Note the long-term long afterglow luminous powder in the coating injection screen printing ink application: 1, use a neutral or weak acidic transparent resin. 2, avoid using metal container storage device, the length of time, depending on how much water content, it will absorb moisture in the air. Should pay attention to moisture, moisture is too heavy to be white, caked. 3, to reduce the luminous paint, luminous powder sedimentation problem, must use high viscosity resin, and adding anti settling agent, the use of the former should stir evenly, use thinner to adjust viscosity, do not use heavy metal compound as additive. 4, printing background use white or reflective colors, can be